Tried this combo last night using the non-aerosol BSI accelerator in a sure shot atomizer and some regular white paper towel
It cured "fine" on the spectraply that finished (sanded to 2000 dry, then buffed).
I have NO idea if this combination:
I am merely reporting what I have witnessed over the last 12 hours with one pen. I did wait 2 minutes between applications and didn't sand until 10 hours later (I do that no matter what CA I use).
PS. If I was repairing one of my guitars, I would only use their accelerator.
It cured "fine" on the spectraply that finished (sanded to 2000 dry, then buffed).
I have NO idea if this combination:
- Will work with all materials
- Last as long as the GB product
- Eventually crack, haze, explode, etc
- Will ever achieve all of the properties that GB is formulated to produce (flexibility, UV protection, hardness, transparency, etc.)
- Will do anything else that you experience when using GB accelerator
- Expand or reduce my carbon footprint
I am merely reporting what I have witnessed over the last 12 hours with one pen. I did wait 2 minutes between applications and didn't sand until 10 hours later (I do that no matter what CA I use).
PS. If I was repairing one of my guitars, I would only use their accelerator.