I am new to this so here goes I turned a pen out of some osage orange
we call it hedge in Kansas but any way The wood came from a barn and is 100+years. We tore the barn down. The pen was a slimline and it turned out nice the next day i was looking at it and it had hairline cracks all over it What caused it?
1 did i turn it to fast and made it hot?
2 Does the wood need stabilized?
I used a CA finish on it. Any ideas?