rblakemore
Member
I am having trouble with some of my wood pens cracking after several months. These have been mainly Kingwood, a really nice color, but straight grain; and, snakewood, which seems to be less straight grain. I was using CA glue, can this be due to an uneven glue coat and uneven contraction/expansion of the wood due to heat and humidity changes??