I seem to be struggling more and more with this.
My method of madness is sand blank to 2000 grit sandpaper. Put on some mineral spirits and let dry. Then 4-6 coats of thin CA with BLO on paper towel. The first coat I give the blank a good coat of BLO to clean dust out and the other coats I just use a few drops. I then sand with 1000, 1200, 1500 sandpaper and then 4000-12000 micromesh.
My problem is that I am getting flat spots in the finish. It seems to be under the surface of the finish if that makes sense.
Somethings I have thought about that might not help the finish.
1. I do not let the BLO totally dry between coats. CA is dry though
2. I don't let the blank site for a few hours to cure before I sand.
3. I might be creating to much heat when sanding the finish.
If anyone has and clues to my problem I would greatly appreciate it. It if very frustrating when I get so far on a pen and the finish looks like crap.
Thanks
Chris
My method of madness is sand blank to 2000 grit sandpaper. Put on some mineral spirits and let dry. Then 4-6 coats of thin CA with BLO on paper towel. The first coat I give the blank a good coat of BLO to clean dust out and the other coats I just use a few drops. I then sand with 1000, 1200, 1500 sandpaper and then 4000-12000 micromesh.
My problem is that I am getting flat spots in the finish. It seems to be under the surface of the finish if that makes sense.
Somethings I have thought about that might not help the finish.
1. I do not let the BLO totally dry between coats. CA is dry though
2. I don't let the blank site for a few hours to cure before I sand.
3. I might be creating to much heat when sanding the finish.
If anyone has and clues to my problem I would greatly appreciate it. It if very frustrating when I get so far on a pen and the finish looks like crap.
Thanks
Chris