Cast #9, almost doubled the pigment

Signed-In Members Don't See This Ad
See more from Drstrangefart

Drstrangefart

Member
Joined
Sep 15, 2010
Messages
4,258
Location
Woodstock, Ga. U.S.A.
318425_220611981332208_100001502242963_590372_744216226_n.jpg


313479_220612047998868_100001502242963_590373_679525260_n.jpg


I let my oldest one pick a couple of colors out, and I probably came really close to using WAAAY too much pigment, just to see what would happen. Still set up well and turned really well. Getting the hang of the changes I made in my finishing, too.
 
Signed-In Members Don't See This Ad
Looks great. You keep it up and Jonathon will be going to the Georgia meetings to get your seconds.
 
looks good. I am waiting on our michaels to get the casting resin in so I can give it a try. any tips.

Make molds around existing blanks out of aluminum foil, cast one blank at a time, and you'll likely need 8 or 9 drops of catalyst per half blank. Use tiny cups like they give you at the dentist's office to mix in, and use popsicle sticks to scoop out pigment and stir.
 
looks good. I am waiting on our michaels to get the casting resin in so I can give it a try. any tips.

Make molds around existing blanks out of aluminum foil, cast one blank at a time, and you'll likely need 8 or 9 drops of catalyst per half blank. Use tiny cups like they give you at the dentist's office to mix in, and use popsicle sticks to scoop out pigment and stir.

Now I'm curious, will you post a pic of your next aluminum foil mold?
 