So Cool an amazing job....What about anodizing the aluminum blue?![]()
Great looking pen - Is it challenging turning aluminum?
Aluminum, to me, is like TruStone in a way. What I have found is there is a lot more chatter when turning. If someone knows a cure I'm all ears. Other than that its real messy to finish. Wet sand with either H2O or 10W40. Either way you get a gray messy liquid that splatters everywhere. I got the satin finish by accident trying to get a shiney finish using 400 grit steel wool then top off with Ren wax. This worked for me I'm sure there are a lot more ideas out there.