watch_art
Member
So the other night I was turning that gray material - rhino plastic (polyresin) - and I kept getting little pits and blisters, but only in one spot on the middle of the barrel. No change in pressure or angle or anything I could think of made a difference. So I turned the lathe off and SMASHED it. Boy that felt good.
THe next night I was turning the brown acrylic, and had the barrel nearly finished. I was turning the end of the barrel to size in the collet chuck and the barrel just split in half. I must have been too aggressive with the skew. Oh well. Happens.
So I used the brown section and put it with some purple russet potato skin lookin plastic. They don't go together too well, but I'm thinking that whoever gets it (a student) won't mind too much.





http://www.fountainpennetwork.com/forum/index.php?app=gallery&module=images&img=1269







http://www.fountainpennetwork.com/forum/index.php?app=gallery&module=images&img=1269