MIKL
Member
my next set of PC pens
the first 2 are slims, it is very hard, well maybe impossible (for me that is) to make PC slims that are true to bushings, i had to turn off a bit of the PC to get them even close, even now they are slightly bulged, thems the breaks
the last is a baron(ess), still very hard to get close to the bushings prior to putting it on the lathe, i didn't take the tools to this one just wet and dry
all are sanded to 12000, then 6 coats of CA for added protection
as per normal SWMBO is trying to swipe them all
thanks for looking
MIK
the first 2 are slims, it is very hard, well maybe impossible (for me that is) to make PC slims that are true to bushings, i had to turn off a bit of the PC to get them even close, even now they are slightly bulged, thems the breaks
the last is a baron(ess), still very hard to get close to the bushings prior to putting it on the lathe, i didn't take the tools to this one just wet and dry
all are sanded to 12000, then 6 coats of CA for added protection
as per normal SWMBO is trying to swipe them all
thanks for looking
MIK
Attachments
-
156 - Slimline - Polymer Clay aedt.JPG256.4 KB · Views: 144
-
156 - Slimline - Polymer Clay bedt.JPG257 KB · Views: 114
-
157 - Slimline - Polymer Clay aedt.JPG259.6 KB · Views: 127
-
157 - Slimline - Polymer Clay bedt.JPG258.7 KB · Views: 97
-
158 - Baron - Polymer Clay aedt.JPG257.7 KB · Views: 142
-
158 - Baron - Polymer Clay bedt.JPG258.5 KB · Views: 125