My first Gentleman's pen. Spalted Ash on Titanium RB hardware. Vacuum stabilized with plexi. My first attempt at spalted Ash was with poly and it literally crumbled apart when I tried to apply the finish.
The blank gained significant weight and the smell of plastic was prominent when I redrilled, but it wasn't as plasticy (new word) as I thought it would be. Turned more like most any other wood, but it stayed together quite well. Only had to CA a few places. BLO/CA finish because by the time I got to MM 12000 it no longer had a wood feel. Very curious indeed, this plexi stabilization stuff.